How To Improve The Transparency Of Plastic Products?

Apr 02, 2020

Leave a message

Because of its light weight, good toughness and easy forming. With the advantages of low cost, more and more plastics are used to replace glass in modern industry and daily products, especially in optical instruments and packaging industry. However, due to the requirements of better transparency, wear resistance and impact toughness, the composition of plastic, the whole process of injection molding process, equipment. A lot of work should be done to ensure that the plastic used to replace glass (hereinafter referred to as transparent plastic) has good surface quality, so as to meet the requirements of use.

 

At present, the transparent plastics commonly used in the market are polymethylmethacrylate (commonly known as acrylic or plexiglass, code PMMA) and polycarbonate (Code PC). Polyethylene terephthalate (PET), transparent nylon. As (acrylonitrile styrene copolymer), polysulfone (PSF) and so on, PMMA is the most exposed one. Due to the limited space of PC and pet, we will take these three plastics as an example to discuss the characteristics and injection process of transparent plastics.

 

1, Properties of transparent plastics

Transparent plastics must first have high transparency, then have certain strength and wear resistance, can resist impact, heat-resistant parts are better, chemical resistance is better, water absorption is smaller, only in this way can they meet the requirements of transparency and remain unchanged for a long time. PC is an ideal choice, but due to its expensive raw materials and difficult injection molding process, PMMA is still the main choice (for products with general requirements), while PPT is mostly used in packaging and containers because it needs to be stretched to get good mechanical properties.

 

2, Common problems in the injection process of transparent plastics

Due to the high transmittance of transparent plastics, the surface quality of plastic products is required to be strict, without any stripes, pores and whitening. Fog halo, black spot, discoloration, poor gloss and other defects, so in the whole injection process of raw materials, equipment. Mold, even product design, should pay attention to and put forward strict or even special requirements.

Secondly, because transparent plastics have high melting point and poor fluidity, in order to ensure the surface quality of products, it is often necessary to adjust the process parameters, such as barrel temperature, injection pressure and injection speed, so that the injection of plastics can not only fill the mold, but also produce internal stress and cause deformation and cracking of products.

In terms of equipment and mold requirements, injection molding process and raw material handling of products, the following points should be noted:

dry

The preparation and drying of raw materials may affect the transparency of the product due to any impurity in the plastic. Therefore, they are stored and transported.

In the process of feeding, attention must be paid to sealing to ensure that the raw materials are clean. In particular, the raw material contains moisture, which will cause deterioration of the raw material after heating, so it must be dried, and when injection molding, the feeding must use a drying hopper. It should also be noted that in the drying process, the input air should be filtered and dehumidified to ensure that the raw materials will not be polluted.

Cleaning of barrel, screw and its accessories

In order to prevent the pollution of raw materials and the existence of old materials or impurities in the screw and its accessories, especially the resin with poor thermal stability, the screw cleaning agent shall be used to clean all parts before use and after shutdown, so that no impurities can be adhered to them. When there is no screw cleaning agent, PE, PS and other resins can be used to clean the screw.

When the machine is shut down temporarily, in order to prevent the raw materials from staying at high temperature for a long time, which will lead to the degradation, the temperature of the dryer and the barrel should be reduced, such as the temperature of PC, PMMA and other barrels should be reduced to below 160 ℃. (hopper temperature shall be below 100 ℃ for PC)

Problems in mold design (including product design)

In order to prevent backflow or uneven cooling from causing poor plastic forming, surface defects and deterioration;

Generally, the following points should be paid attention to in the mold design:

The wall thickness shall be uniform as far as possible, and the angle of demoulding shall be large enough;

The transition should be gradual. Smooth transition to prevent sharp corners. Sharp edges, especially PC products must not have gaps;

Gate. The flow channel shall be as wide and short as possible, and the gate position shall be set according to the contraction and condensation process, and the cold charging well shall be added if necessary;

The mould surface should be smooth and low roughness (preferably less than 0.8);

Vent. The tank must be sufficient to discharge the air and the gas in the melt in time;

Except pet, the wall thickness should not be too thin, generally not less than LMM.

Problems in injection molding process (including requirements of injection molding machine)

In order to reduce the internal stress and surface quality defects, the following problems should be paid attention to in the injection molding process:

Special screw and injection molding machine with separate temperature control nozzle shall be selected;

The injection temperature should be higher when the plastic resin does not decompose;

Injection pressure: generally high, to overcome the defects of high viscosity of the melt, but too high pressure will produce internal stress, resulting in the difficulty and deformation of demoulding;

Injection speed: in the case of mold filling, it should be generally low, and it is better to adopt slow fast slow multi-stage injection;

Pressure holding time and forming cycle: under the condition that the product is filled with mould and there is no depression or bubble, it should be as short as possible to minimize the residence time of molten material in the barrel;

Screw speed and back pressure: on the premise of meeting the plasticizing quality, they should be kept as low as possible to prevent the possibility of falling off;

Mold temperature: the cooling quality of the products has a great impact on the quality, so the mold temperature must be able to accurately control its process, and the mold temperature should be higher if possible.

 

 

Send Inquiry
Contact us if have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!