Causes Of Uneven Shrinkage Of Injection Molded Parts?

Apr 09, 2020

Leave a message

If the plastic parts shrink unevenly, the distribution of internal stress is often uneven. If the stress exceeds the rigidity of the plastic part, it will cause warpage and deformation of the plastic part, and affect the dimensional stability of the plastic part.

 

There are four reasons for uneven contraction:

1. Different melting temperature: the higher the melting temperature, the larger the shrinkage

2. Different cooling speed

Reason: cooling speed is fast < cooling speed is slow (reason: molecules with slow cooling speed have time arrangement, so the shrinkage is large)

3. The flow direction of melt glue is different (amorphous material): in short, the tensile internal stress along the flow direction is large, so the shrinkage is large. In the filling process of plastics, because of the flow orientation, the molecular chain has the phenomenon of orientation. The stretching of the aligned polymer chain in the flow direction and the vertical flow direction is different, which makes the shrinkage behavior different. It is called directional shrinkage.

 

Generally speaking, the in flow shrinkage is higher than the cross flow shrinkage. This is due to the fact that the plastic polymer chain in the flow direction is stretched seriously, and the tendency to return to the unextended state is relatively large. Due to the different shrinkage caused by flow direction, the warpage of plastic parts is often caused. Therefore, if the molecular coordination can be broken up, it will help the uniformity of contraction and reduce the warpage caused by directional contraction. 

 

4. Warping area caused by design: wall thickness

In the area with thick meat, it is difficult to cool and keep pressure, and the cooling time is longer, so the effect of keeping pressure is poor. After demoulding, keep local high temperature and keep cooling. Therefore, in the part with thick meat, such as rib, it is easy to have the phenomenon of local shrinkage causing the plastic part to have a sink mark. Therefore, for the plastic parts with workpiece changes, the selection of pouring position in the thicker position can be conducive to pressure maintaining. Even if the workpiece solidifies, the pressure maintaining pressure can be transferred smoothly to improve the shrinkage phenomenon.

 

Wall thickness variation

Even thickness of plastic parts will improve shrinkage. If the thickness distribution of plastic parts is uneven, it should be considered whether the shrinkage difference caused by different cooling and pressure maintaining effects will cause warpage and deformation of plastic parts, and the problem of stress concentration in the wall thickness transition regions

The phenomenon of internal stress concentration in the transition zone (buffer zone) will cause short-term or long-term warpage and reduce the mechanical performance of plastic parts. Reinforcing rib can be introduced into plastic parts to strengthen structural strength and reduce shrinkage.

The contact part between rib and plastic part wall should be large enough to slow down the stress concentration and overcome the flow resistance, but attention should also be paid to the possible sink mark problem. Generally speaking, the dent size is also affected by the plastic shrinkage characteristics. Considering the strength and rigidity, if the core out method can be used to reduce the thickness of the plastic part, it will help to reduce the shrinkage.

Forming conditions and deformation

 

As the forming conditions related to deformation, special attention must be paid to injection and holding time, cooling time, injection speed and mold temperature.

1. Injection and holding time

The total time of injection and pressure holding is designed to be longer than the gate closing time. If it is shorter than the gate closing time, the deformation sometimes increases.

2. Cooling time

Generally speaking, prolonging the cooling time will reduce the deformation.

3. Injection speed

According to the different shapes of the molded products, sometimes the injection speed is fast, the deformation is small; sometimes the injection speed is slow, the deformation is small. In the actual molding, the minimum deformation condition should be found by changing the injection speed.

4. Mold temperature

Molding products with low mold temperature have small deformation. However, if the use temperature of the molded products is high, sometimes there will be problems of post shrinkage deformation or size change. The mold temperature should be determined according to these factors.

 