After the melt isinjected into the cavity, a thin case is formed on the wall of the die cavity. When the watch case is extruded by the subsequent molten materials in the filling process, the melt will break.
Once the very thin case is torn or moved, the surface of the plastic parts will produce rubbing marks or wrinkles. For example, in low density polyethylene (LDPE) plastic parts with low melt index, a strip area with alternating light and shade can be seen on its surface diameter, and the parts generated are generally at a certain distance from the gate and spread over the whole surface, especially for the thin-walled plastic parts. This is mainly due to the greater pressure on the melt before filling the small melt cavity, which leads to melt fracture, Form surface defects.
Generally speaking, slowing down the cooling rate of molten metal and the formation rate of watch shell layer is the best way to eliminate this kind of fault, which can be eliminated by appropriately increasing the mold temperature or increasing the local temperature of melt fracture. For the local heating of the cavity surface, the small tubular electric heater installed near the gate and the melt fracture site can be used to realize the local heating.
The flow characteristics of the melt are related to its rheological properties, and also to the cross-sectional area of the gate which determines the shear rate at the entrance of the mold. When the size of the gate is small and the injection rate is high, the melt is injected into the cavity with a thin and curved jet flow. If the cooling rate of the melt is very fast, it will not fuse with the irregular flow of the subsequent filling, resulting in surface turbidity and mottling near the gate. Sometimes, a small amount of cold material will move along the surface of the mold cavity, resulting in surface turbidity and mottling at a distance from the gate.
Generally, it is difficult to eliminate the surface turbidity and speckles produced during injection of crystalline polymer, because the melting temperature of this kind of resin is quite high. Compared with amorphous polymer, crystalline polymer has faster curing speed and narrow processing temperature area. Besides, irregular flow occurs at the sharp change of wall thickness and sudden change of melt flow direction, and the melt melts with other melts in the mold cavity It is easy to produce surface turbidity and mottling.
In order to eliminate this kind of fault, the temperature of mould, barrel and nozzle should be raised properly, and the advance speed of screw during injection should be reduced.
In the mold operation, the gate size should be enlarged, and the fan-shaped gate should be preferred. If the tunnel gate is used, its top size will be too small, which will affect the mold filling and aggravate the irregular flow of the flowing material. The top size should be appropriately increased; if the mold exhaust is not good, it will also affect the regular flow of the flow material, which should be improved. In addition, the amount of lubricant should be reduced and the suitable variety should be selected.