Ten Processing Skills Of Injection Molding - Mould Scale Of Products

Feb 01, 2020

Leave a message

Almost all thermoplastics have this problem. Due to the increasing requirements for the finished products, the requirements for the addition of modifiers, flame retardants and other additives are correspondingly increased. These additives often produce mold scale on the surface of the mold cavity.

There are other reasons that may cause mold scale during molding.

Some of the most common reasons are:

Thermal degradation; excessive shear; inadequate exhaust

The formation of these scale is usually caused by the comprehensive action of different factors. It is necessary to find out the faults and analyze the causes and prevention methods of mould scale. The problem is that mold scale usually does not appear until a few days later

Type of deposition

Each type of additive produces a specific type of scale. The flame retardant can degrade at high temperature, and the degradation products may form scale. The impact modifier is not only affected by high temperature, but also by excessive shear. Under unfavorable conditions, the modifier can be separated from the plastic and form mold scale on the surface of the mold cavity.

Engineering plastics need pigments with high melting temperature. These pigments can reduce the thermal stability of special materials for engineering plastics. As a result, mold scale composed of degradation products of plastics and decomposition products of pigments is produced

Some parts of the mold are particularly hot (e.g. mold), modifiers / stabilizers and other additives may stick to the surface to form mold scale. In this case, certain steps must be taken to improve the temperature control of processing and molding, or use special stabilizer. The possible causes of mould scale and the methods to prevent it are listed in the table.

Sudden appearance

If mold scale suddenly occurs, it may be that the conditions of molding process have changed, or different batches of plastics have changed. The following comments may help.

First of all, in order to find mold scale, the melt temperature should be measured, and eyes should be used to check whether there are signs of material decomposition, such as whether there are particles burnt by the material. You can check whether the plastic is contaminated by foreign substances, whether the cleaning materials are incompatible with the materials, and also check the exhaust of the mold. The next step is to use primary or color (non black) plastic. After the machine has been running for about 20 minutes, shut down the machine, dismantle the nozzle, head and even screw. Checking the composition of the coking particles and comparing their color with the original plastic will soon find out the source of the problem.

In some cases, this technique will expose some unexpected problems, but it is only applicable to small machines (i.e. injection molding machines with screw diameter no more than 40mm). The elimination of these problems will improve the quality of other materials to a certain extent. Similar procedures apply to hot runner machines.

Mold maintenance

If the method described above cannot prevent the formation of mould scale, special attention shall be paid to the mould.

It has been found that the scale on the surface of the cavity is relatively easy to remove at the early stage of its formation. Therefore, the cavity and vent should be cleaned at specific intervals, such as at the end of each shift. Once the mold scale is thick, it will be very difficult and time-consuming to remove it.

Because the chemical composition of scale varies greatly, many experiments must be carried out to determine the most suitable solvent. In addition to traditional solvents, some non-traditional products can also solve this problem, such as oven spray or lemonade containing caffeine. Another method is to use clean rubber for traditional model railway

Suggestions to prevent scale formation

If you use a hot runner mold to process thermosensitive plastics, remember that in this case, the material will stay in the mold for a long time, so the possibility of mold scale due to material decomposition is greater.

The plastic sensitive to shear should be processed with large-scale runner and gate mold. Multi - point gate will reduce the flow distance, thus can reduce the injection speed and achieve better results

Generally speaking, the effective exhaust during the molding process can reduce the possibility of mold scale formation. When designing the die, we should pay attention to providing sufficient vent holes. It is better to use self-cleaning vent or mould scale capacity as the vent for cleaning. The improvement of the exhaust system often reduces the mould scale in the mould

In some cases, it may be necessary to apply a special non stick coating on the cavity surface to prevent the formation of mold scale, and tests shall be carried out to evaluate the effectiveness of the coating. Titanium nitriding often reduces the rate of fouling in the mold

 

Send Inquiry
Contact us if have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!