Causes And Solutions Of Insufficient Opening Force Of Injection Molding Machine

Jun 30, 2020

Leave a message

1. The area of open die oil pressure ring is too small

Opening force = area of opening oil pressure ring × opening oil pressure

Under the condition of the highest pressure, if we want to increase the opening force, we can only increase the area of the opening oil pressure ring by increasing the diameter of the oil cylinder or reducing the diameter of the piston rod.

2. Too small clearance of opening oil

In the first section of the die opening, because the fit clearance between the hydraulic buffer sleeve and the inner hole of the front cover of the oil cylinder is too small, the pressure oil is slow and even difficult to enter the die opening cavity of the oil cylinder, so the maximum die opening force cannot be provided.

Increase the fit clearance between the hydraulic buffer sleeve and the inner hole of the front cover of the oil cylinder, so that the pressure oil can quickly enter the opening cavity of the oil cylinder and form the opening force with a certain amount of punch, which may cause certain impact during the opening.

3. When the angle of θ exceeds 90 ° after high pressure die locking, the reverse hinge will be caused

The designof hinge parameters, the stroke and installation position of die locking cylinder determine the end position of small hinge and form a θ angle during the final high-pressure die locking. The designed θ angle must ensure that the θ angle of the machine installed within the accumulated tolerance range of each part processing is absolutely less than 90 °.

Once the angle of θ exceeds 90 °, the small hinge appears reverse hinge. At this moment of opening, the hook hinge and long hinge actually rely on the straight direction to produce greater clamping force. Finally, the small opening force is not enough to overcome the deformation force caused by increasing the clamping force, so the opening moment cannot be completed.

774835576b7e4bd9a22d83013865cd6e.gif

4. Too much deformation force can not be overcome by opening force

When the hinge of the machine is designed, the amplification ratio of the hinge when it produces the established locking force has been determined. Based on this, the thrust of the required locking cylinder can be designed to determine the diameter of the locking cylinder. The cylinder should also have enough opening force. If the opening force is sufficient, the larger the diameter of the cylinder, the better.

But the too large diameter of the oil cylinder leads to the too large thrust of the oil cylinder when the mold is locked, which leads to the overload of the mold locking force (when the mold is not adjusted well), the deformation force of the hinge is too large, and the mold opening force cannot overcome the too large deformation force, which leads to the failure of the mold opening.

In this case, the overload of clamping force can be prevented by limiting the high-pressure clamping pressure and flow. When adjusting the mold, be patient and use the lower clamping pressure as much as possible to transfer out the shared clamping force.

5. Low opening pressure and small flow lead to small opening punch

Because of the low opening pressure and small flow, the small opening punch is unable to overcome the deformation force of the hinge, especially the small flow of the first section of the opening die provided by the servo control system, the small opening punch is more difficult to open the die.

This problem can be solved by modifying the PID and the slope of the controller.

acea9f0b0aa843dcbf5887561e264f3e.jpg

6. It is difficult to open the mould due to the temperature rise after the pressure test

After a period of time of pressure test, the temperature of the die increases and the die locking force increases, which makes it difficult to open the die. Pay attention to adjust the plastic modulus in time to make the locking force return to the original value, so as to avoid mold failure.

7. Too long shutdown time after mold locking, resulting in failure to open mold

After the die is locked, the shutdown time is too long, which leads to the complete disappearance of the lubricating oil film of the hinge and the further increase of the deformation of the hinge, resulting in the inability to open the die.

Therefore, try to reduce the downtime of mold locking. Before the shutdown, remember to open the mold, and do not shut down the machine when the mold is locked.

8. Back pressure of die opening leads to insufficient punch

Setting the back pressure of the opening section on the oil circuit also leads to the deficiency of the opening punch. If this situation is found, the back pressure of the opening will be cancelled.

9. The friction resistance in the hinge is too large, which leads to the opening resistance

The friction resistance between the large pin shaft and the steel sleeve in the hinge is too large, which leads to the need for greater opening force to overcome its friction resistance:

(1) The oil groove edge in the steel sleeve is not deburred, which causes the burr to wear into particles and enter into the mating surface of the big pin shaft and the steel sleeve, and causes the mating surface to wear or burn the mating surface.

In order to avoid this problem, it is required to deburr and smooth these parts after processing. During installation, check again and clean all surfaces and apply lubricating grease before installation.

(2) If there is insufficient lubrication or lubrication failure, it will also lead to excessive friction resistance. At this time, check whether the lubricating oil circuit is normal and whether the lubricating pump is normal.

 